鎂質和鎂鉻質搗打料選用優質鎂砂和鎂鉻材料經粒度配比加入各種結合劑、促凝劑和燒結劑制成。特點:強度高,整體性好,高溫下體積穩定性強。是各種工業窯爐保溫、隔熱、密封的理想材料。 |
|
|
|
|
牌 號
|
MGe
|
MRD-1
|
MRD-2
|
MRD-3
|
MRD-4
|
MRD-5
|
|
最高使用溫度(℃)
|
1600
|
1750
|
≥1750
|
1700
|
≥1700
|
≥1700
|
|
化學成份
(%)
|
MgO
|
58.61
|
≥94
|
95
|
93
|
95
|
95
|
|
Cr2O3
|
17.36
|
---
|
---
|
---
|
---
|
---
|
|
CaO
|
0.73
|
≤2.0
|
---
|
≤2.0
|
---
|
---
|
|
SiO2
|
4.17
|
≤1.0
|
≤3.0
|
≤3.0
|
---
|
---
|
|
線變化率
(%)
|
110℃×24h
|
---
|
---
|
---
|
-1.0/+0.2
|
-0.1
|
---
|
|
1000℃×3h
|
+0.3/0.1
|
---
|
---
|
---
|
---
|
---
|
|
1600℃×3h
|
-0.25/-0.50
|
---
|
---
|
-0.70/1.0
|
-0.4/0.8
|
-0.3
|
|
耐壓強度
(Mpa)
|
20
|
13.01
|
---
|
---
|
---
|
---
|
---
|
|
110℃×3h
|
---
|
40
|
40
|
30
|
70
|
60
|
|
1000℃×3h
|
7.14
|
---
|
---
|
---
|
---
|
---
|
|
1600℃×3h
|
10.17
|
30
|
20
|
50
|
60
|
60
|
|
體積密度
|
100℃×24h
|
---
|
2.9
|
2.8
|
2.7
|
2.9
|
2.8
|
|
1600℃×3h
|
---
|
---
|
---
|
2.78
|
2.85
|
2.90
|
|
容 量
|
|
>3.0
|
---
|
---
|
---
|
---
|
---
|
|